Polymer Property : Flexural Modulus = 1.40 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.00 - 1.40 GPa
145 - 203 ksi
from bending test; DIN 53 457
Hippe PE 300 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
Flexural Modulus 0.450 - 1.40 GPa

@Temperature 60.0 - 120 °C
65.3 - 203 ksi

@Temperature 140 - 248 °F
Average value: 0.883 GPa Grade Count:1
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..