Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.647 - 0.686 GPa | 93.8 - 99.5 ksi | ASTM D790 |
Daikin NEOFLON AP-210AS PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for injection molding.Information provided by D.. |
|||
Flexural Modulus | 0.647 - 0.686 GPa | 93.8 - 99.5 ksi | ASTM D790 |
Daikin NEOFLON AP-230ASL PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for extrusion molded parts. Piping, tube, etc... |
|||
Flexural Modulus | 0.647 - 0.686 GPa | 93.8 - 99.5 ksi | ASTM D790 |
Daikin NEOFLON AP-201 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Complicated injection molded parts requiring high melt flow to fil.. |
|||
Flexural Modulus | 0.647 - 0.686 GPa | 93.8 - 99.5 ksi | ASTM D790 |
Daikin NEOFLON AP-210 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Injection molded parts, wire insulation, etc.Information provided .. |
|||
Flexural Modulus | 0.647 - 0.686 GPa | 93.8 - 99.5 ksi | ASTM D790 |
Daikin NEOFLON AP-230 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |