Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.600 - 0.600 GPa @Temperature 90.0 - 90.0 °C |
87.0 - 87.0 ksi @Temperature 194 - 194 °F |
Average value: 0.600 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Flexural Modulus | 0.462 - 0.600 GPa | 67.0 - 87.0 ksi | ASTM D790 |
Buckeye Polymers BP FLEX D0850(C) BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Flexural Modulus | 0.600 - 0.600 GPa @Temperature 90.0 - 90.0 °C |
87.0 - 87.0 ksi @Temperature 194 - 194 °F |
Average value: 0.600 GPa Grade Count:1 |