Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.70 GPa | 1410 ksi | ASTM D790 |
Premix Premi-Glas® 3101-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-15 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | ASTM D790 |
Resinoid 2215 Phenolic Molding, Cellulose Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Flexural Modulus | 9.70 GPa @Temperature 23.0 °C |
1410 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Rynite® RE19051 BK507 PET
(Unverified Data**) Rynite® RE19051 BK507 is a 40% glass and mineral reinforced, flame retardant, polyethylene terephthalate black resin.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | ASTM D790 |
Plenco 5303 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 5303 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in appliance, automotive and electrical applications. It can be molded by compression, transfer or i.. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66 LNP* LUBRICOMP* RFL36XXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66 (Asia Pacific) LNP Lubricomp is a compound based on PA66 resin containing glass fiber, PTFE. It is an internally lubricated compound that provide excellent chemical resistance, strength and wear/friction propertie.. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features include: Electrically Conductive, Easy Molding, Mold Release. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF006S PA 66 LNP* THERMOCOMP* RF006S is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA 6/10 LNP LUBRICOMP* QFL36 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | ASTM D790 |
Solvay TECHNYL® 2412GHF6 PA66, 33% glass fiber, DRY Description: Polyamid 66, reinforced with 33% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF6 is used in all sectors of indu.. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | ISO 178 |
Polyplastics Duranex® C5330 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | ISO 178-93 |
Wellman Wellamid® GF33A099-HRN Nylon 66, 33% Glass Reinforced, Hydrolysis Resistant All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | ASTM D790 |
Toyobo VYLOPET® EMC330 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | ISO 178 |
DuPont Performance Polymers Rynite® RE19051 BK507 Polyethylene Terephthalate (PET) 40% Glass/Mineral Reinforced Flame Retardant Polyethylene Terephthalate Rynite RE19051 BK507 is a 40% glass and mineral reinforced flame retardant polyethylene terephthalate black resin.Information .. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | ASTM D790 |
Adell BR-38 Nylon 6, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | ASTM Test |
BASF Petra® 130 FR 30% Glass Filled PET Petra 130 FR is a 30% glass fiber reinforced, flame retardant injection molding polyethylene terephthalate feedstocks. It is recognized as UL 94V-0/5VA by Underwriters Laboratories. It is also avail.. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | ASTM Test |
BASF Petra® 130 FR BK-112 30% Glass Filled PET Petra 130 FR BK-112 is a 30% glass fiber reinforced, black pigmented, flame retardant injection molding compound based on post-consumer and post-industrial recycle polyethylene erephthalate feedstoc.. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 514 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 9.70 GPa | 1410 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |