Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.85 GPa | 1280 ksi | 1.3 mm/min; ASTM D790 |
Ovation Polymers Opnyl OP66GF43 Nylon 66, Dry as Molded Nylon 66-Glass reinforced(43%), high tensile strength, stiffness and HDT.Information provided by Ovation Polymers |
|||
Flexural Modulus | 8.85 GPa | 1280 ksi | ISO 178-93 |