Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.21 GPa | 1190 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE0021E PC LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding, Flame Retardant, Electrically Conductive. |
|||
Flexural Modulus | 8.21 GPa | 1190 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE0021E PC (Asia Pacific) LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 8.21 GPa | 1190 ksi | ISO 178 |
SABIC Innovative Plastics LNP VERTON PX00700 PA 6 LNP VERTON* PX00700 is a compound based on Nylon 6 resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Flexural Modulus | 8.21 GPa | 1190 ksi | ISO 178 |
SABIC Innovative Plastics LNP VERTON PX00700 PA 6 (Asia Pacific) LNP* Verton* PX00700 is a compound based on Nylon 6 resin containing Long Glass Fiber. |