Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP FARADEX KX98009 Acetal Copolymer (Europe-Africa-Middle East) LNP* FARADEX* KX98009 is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber, Glass Fiber. Added features include : EMI / RFI Shielding, Electrically Conductive. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ISO 178 |
Wellman Wellamid® GFT33N051-N2 33% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized
&n Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
Plenco Valite 4100 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability charac.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ISO 178 |
Kuraray Genestarâ„¢ G1301A-M61 Nylon, 30% Glass Filled 30% Glass reinforced and impact modified injection grade.Main Features:Higher elongation and impact strengthHeat resistanceChemical resistanceExample of applications:Quick connector |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon WC003 PBT (Europe-Africa-Middle East) LNP* Stat-kon* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP JX97000 PES (Europe-Africa-Middle East) LNP* Thermocomp* JX97000 is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Mold Release. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP KF004 Acetal Copolymer LNP THERMOCOMP* KF004 is a compound based on Acetal Copolymer resin containing 20% Glass Fiber. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp PF006 PA 6 (Asia Pacific) Nylon 6 compound containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF0067K PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF0067K is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 226F6T3 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6T3 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It shows its high mechanical strength over a long period and is able to perform at higher.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ISO 178 |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
Unitika AXG-1500-300 Dry Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
Plenco 4485 Phenolic, Granular, Compression Molded PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ISO 178 |
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM-D790 |
Polyram Polytron P40B01 Homopolymer Polypropylene, Chemically Coupled 40% LGF A chemically coupled 40% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GVZ 30 HWCP 30% Glass Fiber Z-Qualities Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790, ISO 178 |
EPICHEM Epiter PBT GF 30 Polybutylene Terephthalate, 30% Glass Characteristics: 30% glass fibre filled |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612 33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GV 30 HWCP 30% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | After conditioning at 23°C and 50% RH; ISO 178 |
Arkema Group Orgalloy® RS 6635 A Polyamide 6.6 Alloy 35% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 283 PPO Alloy, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ISO Value |
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8233G is a 33% glass fiber reinforced polyamide 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also available in he.. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | ASTM D790 |
PlastxWorld CEVIAN® B2506 30% GF PBT/ABS Alloy Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 8.20 GPa | 1190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® VX4930 PBT (Europe-Africa-Middle East) VALOX VX4930 is a 30% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |