Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.04 GPa @Temperature 150 °C |
1170 ksi @Temperature 302 °F |
ASTM D790 |
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Flexural Modulus | 8.04 GPa | 1170 ksi | 5 mm/min; ISO 178 |
Gromax BFG30-DN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 8.04 GPa | 1170 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE003 PC (Asia Pacific) LNP STAT-KON* DE003 is a compound based on Polycarbonate resin containing Carbon Fiber. |
|||
Flexural Modulus | 8.04 GPa | 1170 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE003ER PC LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Statically Conductive. |
|||
Flexural Modulus | 8.04 GPa | 1170 ksi | ASTM D 790 |
SABIC Innovative Plastics Valox® PDR4911 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 8.04 GPa | 1170 ksi | |
Shinil Chemical SHINNANO PA-6 Polymer Nanocomposite Air Intake Module SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Flexural Modulus | 8.04 GPa | 1170 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GP-5300G PBT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 8.04 GPa | 1170 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GP-5300G PBT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 8.04 GPa | 1170 ksi | ASTM D790 |
Samyang Tribit® 1500GN30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |
|||
Flexural Modulus | 8.04 GPa | 1170 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp WF006SXC PBT LNP* Thermocomp* WF006SXC is a compound based on PBT containing Glass FIber. Characteristic of this grade is: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 8.04 GPa | 1170 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE003ER PC (Asia Pacific) LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 8.04 GPa | 1170 ksi | ASTM D790 |
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Modulus | 8.04 GPa | 1170 ksi | ASTM D790 |
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Modulus | 8.04 GPa | 1170 ksi | 5 mm/min; ISO 178 |
Gromax CFG30-QN11N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |