Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.93 GPa | 1150 ksi | Tangent; ASTM D790 |
RheTech Products GC40P100-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | ASTM D790 |
Quadrant EPP Ketron® CM 1030HT PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | ASTM D790 |
LNP Thermocomp® EF-1004 BK8-115 Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 0177 Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10 LNP* THERMOCOMP* QF007 is a compound based on Nylon 6/10 resin containing 35% Glass Fiber. |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | ASTM D790 |
Chase Plastics CP Pryme® A130 ABS, 30% Glass Fiber Reinforced Features: Glass fiber reinforcementInjection moldingForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | ASTM D790 |
A. Schulman LUBRILON® 432 30% Glass Fiber Reinforced, PTFE Lubricated PBT Alloy Information provided by A. Schulman. |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® GFPC-30 30% Glass-Reinforced Polycarbonate Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar.. |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | ASTM D790 |
A. Schulman LUBRILON® 432 30% Glass Fiber Reinforced, PTFE Lubricated PBT Alloy Information provided by A. Schulman. |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | ASTM D790 |
A. Schulman LUBRILON® 432 30% Glass Fiber Reinforced, PTFE Lubricated PBT Alloy Information provided by A. Schulman. |
|||
Flexural Modulus | 7.93 GPa | 1150 ksi | ASTM Test |
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin.. |