Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.74 GPa | 1120 ksi | ASTM D790 |
LG Chemical LUPOY GP-2301F General Purpose Modified PC, 30% Glass Fiber Reinforced, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Flexural Modulus | 7.74 GPa | 1120 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp MF0069S PP LNP* Thermocomp* MF0069S is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant, Heat Stabi.. |