Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.425 GPa | 1077 ksi | ISO Value |
BASF Capron® 8333G HI Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8333G HI is a 33% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance .. |
|||
Flexural Modulus | 7.425 GPa | 1077 ksi | ISO Value |
BASF Capron® 8333G HI HS BK-102 Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8333G HI HS BK-102 is a 33% glass reinforced, impact modified polyamide 6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughness in c.. |