Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.32 GPa | 1060 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66 LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead. |