Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
PolyOne Nymax™ GMF 604 40 UV Black 115 1 X 1 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Nylene® Naxel™ PC506 30% Glass Reinforced Polycarbonate Description: Naxel™ PC506 is a 30% glass fiber reinforced polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resourc.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Nylene® Norpex® AX30GF , 30% Glass Reinforced Polyphenylene Ether Description: Norpex® AX30GF is a 30% glass fiber reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
PolyOne Trilliant™ HC HC3220-0030 RS Natural Polycarbonate (PC) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR15 MF25 Glass/Mineral Filled Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Polymer Resources PPX-FRG30 Modified-PPO, V-1 Flame Retardant, 30% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 30% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Polymer Resources TPSF-FRG30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1240MHL BK Nylon 6/6 Available in North America Filler: Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated, Low Warpage and Heat StabilizedRoHS CompliantForm: Pellets Processing .. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Polymer Resources PPX-FRG30 Modified PPO, UL 94 V-1, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
PolyOne Nymax™ GF 1880 33 HS NATURAL Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedHeat StabilizedMolded Test Bars: (Dry as molded:Information provided by PolyOne Corporation. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES Electrablend® PA12 CF13 L 13% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 13% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and lubricatedInformation provided by TP Composi.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES Electrafil® J-3/CF/10 Nylon 6, 10% Carbon Fiber Reinforced |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF25 FR BK 25% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedAppear.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES HiFill® HIPS GF20 BK 20% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 0190 Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF25 FR NAT003 25% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedUL Fil.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Westlake Plastics Pomalux® 25% GF Acetal Copolymer 25% Glass Filled Pomalux is a high performance acetal copolymer that has excellent mechanical, electrical, and wear properties. It is engineered to provide outstanding dimensional stability, even when machining par.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Asahi Kasei Thermylene® P7-40FG-1804 40% Glass Fiber Reinforced, Chemically Coupled Information provided by Asahi Thermofil |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF25 FR 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightUL File Number: E157318TPCI# 9085101Information provided by TP Composites, Inc. |