Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
PolyOne OnForce™ LFT PP-40LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 3413R PC (Europe-Africa-Middle East) LEXAN 3413R is a high viscosity, 30% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance. |
|||
Flexural Modulus | 7.00 - 9.00 GPa | 1020 - 1310 ksi | Injection; ISO 178 |
Raschig Group DECAL® 1760 Phenolic Glass-fiber reinforced phenolic molding compound. Very good electrical properties, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals an.. |
|||
Flexural Modulus | 7.00 - 9.00 GPa | 1020 - 1310 ksi | Injection and Compression; ISO 178 |
Raschig Group MELOPLAS® 3025 MF Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu.. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
Hexion Bakelite™ X30 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, reinforced with cotton and sisal fibers, increased notched impact strength.Application areas: Covers for electrical and electromagnetic devices.Information provided by Bak.. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | ASTM D790 |
Plenco 307 Black Impact Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 307 is a two-stage, mineral and flock-filled phenolic molding compound designed for the automotive industry for use in brake system components. It is characterized by good molding latitude .. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | |
Lehmann & Voss LUVOCOM® 50-7586 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts with low warpage and.. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | |
Lehmann & Voss LUVOCOM® 80/CF/10/BK Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
Mitsubishi Xantar® G6F 23 UR Polycarbonate-30% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | ASTM D790 |
Loxim 230 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
Solvay TECHNYL® R AR 218 V30 Nylon 66, 30% glass fiber, DRY Description: TECHNYL® AR 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. It contains recycled materials. This product is available in black .. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 830F PBT+PET (Asia Pacific) PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON KE002 Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-kon* KE002 is a compound based on ACETAL COPOLY resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 LNP* STAT-KON* SE003 is a compound based on Nylon 12 resin containing 15% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Asia Pacific) LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UF004AS PPA (Europe-Africa-Middle East) LNP* Thermocomp* UF004AS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178-93 |
Wellman Wellamid® MR410 22H-GY1 40% Mineral Reinforced Nylon 66 Description: Mineral Reinforced Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | D790 |
Zhejiang Juner 302-G30 30% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612 33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Flexural Modulus | >= 7.00 GPa | >= 1020 ksi | IEC 1212-2 5.2 |
Hippe PF CP 201 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical applications. Used in mechanical properties better than other PF CP types. Poor electrical properties under normal humidity. Also available in hot-punching versions.Information.. |
|||
Flexural Modulus | >= 7.00 GPa | >= 1020 ksi | IEC 1212-2 5.2 |
Hippe PF CP 204 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in electrical and electronic applications. Good stability of electrical properties under high humidity. Also available in cold or hot-punching versions.Information provided by Hippe. |
|||
Flexural Modulus | >= 7.00 GPa | >= 1020 ksi | IEC 1212-2 5.2 |
Hippe PF CP 206 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions.Information provided by Hippe. |
|||
Flexural Modulus | >= 7.00 GPa | >= 1020 ksi | IEC 1212-2 5.2 |
Hippe PF CP 308 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions. Flame retardant.Information provided by Hippe. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | ASTM D790 |
E-Polymers TEKAMID® TA210GM , GF/MF Reinforced PA66, DAM GF/MF reinforced, Heat resistance, Low warpageInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | ASTM D790 |
E-Polymers TEKAMID® TA250GM , GF/MF Reinforced PA66, DAM GF/MF reinforced, Good surface, Low warpageInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 7.00 - 10.0 GPa | 1020 - 1450 ksi | ASTM D790 |
Chang Chun Plastic PBT4130 Fire Retardant & 30% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC (Asia Pacific) LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | ASTM-D790 |
Polyram RamSter PF392G6 PBT, 30% Glass Fiber 30% glass-fiber reinforced, surface modified PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON ME003S PP LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized. |