Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.80 GPa @Temperature 90.0 °C |
986 ksi @Temperature 194 °F |
ISO 178, ASTM D790 |
Nilit Nilamid B3 H G8 40% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G8 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key character.. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | 10mm/min; ASTM D790 |
PTS PBT-20GFR 20% Glass Filled PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by PTS LLC. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | 2mm/min; ASTM D790 |
Kingfa PA66-RG201 Flame Retardant, 20% Glass Fiber Reinforced PA66 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesNo bloomingApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation Provided by Kingf.. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ISO 178 |
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH50 Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an.. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ISO 178 |
Solvay TECHNYL® C 216 V35 Black Z PA6, 35% glass fiber, Conditioned Description: Polyamide PA6 , reinforced with 35 % of glass fiber, for injection molding.Available in: North AmericaProduct Applications: It has good mechanical properties, it is used in all sectors .. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ISO 178 |
Solvay TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, DRY Description: TECHNYL® eXten D 238 V30 is a PA6,10 30% glass fiber reinforced and impact modified suitable for injection molding. TECHNYL® eXten D 238 V30 is based on a partially bio-sourced po.. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DC10EPFR PC LNP* STAT-KON* Lexan_DC10EPFR is a compound based on Polycarbonate containing Carbon Fiber. Added features of this grade include: Exceptional Processing, Flame Retardant, Electrically Conductive. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP EF004 PEI LNP* Thermocomp* EF004 is a compound based on Polyetherimide resin containing 20% Glass Fiber. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 126F4RZ21 Nylon 6, 20% Glass Fiber SAXAMID 126F4RZ21 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers. It is equipped with a halogen-free and phosphorus-free flame retardant.Information provided by SAX Polyme.. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp MF006S PP (Asia Pacific) LNP* Thermocomp* MF006S is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia P.. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RFB44XE PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RFB44XE is a compound based on Nylon 66 resin containing Glass Fiber, Glass Bead. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermotuf PF007IX2 PA 6 (Europe-Africa-Middle East) LNP * THERMOTUF* PF007IX2 is a compound based on PA 6 resin containing Glass Fiber. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ASTM D790 |
Plenco 2000 Phenolic, Granular, Injection Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ISO 178 |
Unitika TERRAMAC TE-8210 Polylactic Acid (PLA) High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ASTM-D790 |
Polyram PlusTek PA4801G6 Nylon 6.6, 30% Glass Fiber Reinforced, PTFE lubricated 30% glass fiber reinforced, PTFE lubricated polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ISO 178 |
Polyram RamLloy PZF301G4 PC/PBT Alloy, 20% Glass Fiber 20% Glass fiber reinforced, impact modified PC/PBT alloy for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ASTM D790 |
Plenco 7523 Phenolic, Granular, Transfer Molded PLENCO 07523 is a woodflour and cotton flock filled novolac phenolic molding compound, formulated for high impact industrial uses. UL recognized under component file E40654.Information supplied by P.. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | cond; ISO 178 |
DSM Stanyl® 46SF5030 PA46-GF30 FR(17) 30% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ISO 178 |
Eurostar Staramide 6 70E3 PA6, 70% Mineral Filled, Injection Molded Staramide 6 70E3 is a 70% mineral filled high density, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | 2 mm/min; ISO 178 |
Eurostar Starpylen MF008S PP, 40% Glass Fiber Filled, Injection Molded Starpylen MF008S is a 40% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ISO 178 |
BASF Petra® 7010 WT 7729 15% Glass Filled PET Description: Petra 7010 WT7729 is a 15% glass fiber reinforced, pigmented white injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface .. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ASTM D790 |
Ascend Performance Materials VYDYNE® R400G Nylon, Mineral and Glass Reinforced Typical property data. VYDYNE is a registered trademark of Solutia Inc. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ASTM D790 |
Ashley Polymers Ashlene® D925LH-30G Nylon 12, 30% Glass Reinforced A 30% glass reinforced heat and light stabilized Nylon 12.Data provided by the manufacturer |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | Wet |
Asahi Kasei Leona® 1300G Polyamide 66 Resin, Glass Reinforced Applications: Automotive: Radiator Tanks, Fuel Injectors, ABS Sensors, Engine Mounts Electrical and Industrial: Heater Tanks, Office Furniture, Small EnginesInformation provided by Asahi Kasei |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 212 Polystyrene, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | 10mm/min; ASTM D790 |
BLUESTAR PBT 403M-G20 20% Glass Filled PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 6.80 GPa | 986 ksi | ASTM D790 |
Plenco 7579 Phenolic, Granular, Injection Molded PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40.. |