Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.50 GPa | 943 ksi | STN EN ISO 178 |
Plastcom PLASTAMID® 6 GF 30 031 TS PA6 reinforced with glass fiber, heat stabilized PA 6 for injection molding, reinforced with 30% glass fiber, heat stabilized, better surface appearance of injection moldings. Decrease in tensile strength by 50 % after 5000 hours at 170°C. Used f.. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 66 GF 25 Polyamide 66, 25% Glass Fiber FeaturesChemically reinforced with 25% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | ISO 178, ASTM D790 |
Nilit Nilamid A3 H G4 General Purpose 20% Glass Reinforced PA66 Description: Nilamid A3 H G4 is a general purpose, 20% glass fiber reinforced NYLON 66. This product combine good overall mechanical performance and impact strength with ease of processing.Key chara.. |
|||
Flexural Modulus | 6.50 GPa @Temperature 23.0 °C |
943 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANMID 6 B11^ FX25 FR10 Nylon 6, Glass Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Modulus | 6.50 GPa @Temperature 90.0 °C |
943 ksi @Temperature 194 °F |
ISO 178, ASTM D790 |
Nilit Nilamid A3 H7 G7 35% Glass Reinforced PA66 Description: Nilamid A3 H7 G7 is a 35% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc.. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | ASTM D790 |
NOVA Chemicals Dylark® 250P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Flexural Modulus | 6.50 - 12.1348 GPa @Temperature -40.0 - 120 °C |
943 - 1760.03 ksi @Temperature -40.0 - 248 °F |
Average value: 9.41 GPa Grade Count:2 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | ASTM D790 |
Loxim 130 01HB Polycarbonate, 30% Glass Filled, Flame Retardant Information provided by Loxim Industries |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | ISO 178 |
Grupo Repol Dinalon® A1S25 G25PV0 25% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 66 Mechanical properties are for dry as molded samples.Information provided by Grupo Repol. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 2200 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 2210 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 2210F PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem PW2200 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water
applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and.. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon DE002E PC (Europe-Africa-Middle East) LNP* STATKON* DE002E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features include; Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU), 20% Glass Fiber Veradel® 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | ISO Data |
Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Dry) Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | 3-Point Bending; ISO 178 |
Styron INSPIREâ„¢ DLGF 9621.00 Compounded Polypropylene, 60% LGF Overview: DLGF 9621.00 is a polypropylene homopolymer reinforced with 60% by weight of long glass fiber. PP-LGF60, Long Glassfiber Granulate). DLGF 9621.00 is produced by pultrusion/melt-impregnatio.. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | 3-Point Bending; ISO 178 |
Styron INSPIREâ„¢ DLGF 9631.01 Z Polypropylene homopolymer, 60% LGF Overview: DLGF 9631.01 Z is based on polypropylene homopolymer and reinforced with 60% by weight of long glass fiber. (PP-LGF 60, Long Glassfiber Granulate). DLGF 9631.01 Z is produced by pultrusion.. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp RFB24 PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RFB24 is a compound based on PA 66 resin containing Glass Bead, Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | ISO 178 |
Polyplastics Duranex® 7307 Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | ISO 178 |
Polyram PlusTek PB300G4 Nylon 6 for Injection Molding, 20% Glass-Fiber Reinforced 20% Glass fiber reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | ASTM-D790 |
Polyram RamOfin PPH300G8 Polypropylene, 40% Glass Fiber 40% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 6.50 - 8.00 GPa | 943 - 1160 ksi | ISO 178 |
Vyncolit 2530 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba.. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GVS 10/30 HWCP 10% Glass Fiber and 30% Glass Sphere Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GVS 20/10 HWCP 20% Glass Fiber and 10% Glass Sphere Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | ASTM D790 |
Beijing Ranger Chem PBT-201-G10 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU (Europe-Africa-Middle East) LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing Glass Fiber. |
|||
Flexural Modulus | 6.50 GPa | 943 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, Conditioned Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |