Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.48 GPa | 940 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Flexural Modulus | 6.48 GPa | 940 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive. Wear Resistant, Flame Retardant. |
|||
Flexural Modulus | 6.48 GPa | 940 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC (Asia Pacific) LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 6.48 GPa | 940 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP CX05470 PS LNP* THERMOCOMP* CX05470 is a compound based on Polystyrene resin containing 20% Glass Fiber. |
|||
Flexural Modulus | 6.48 GPa | 940 ksi | |
Asahi Kasei Xyron® G703H Modified Polyphenylene Ether Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P.. |
|||
Flexural Modulus | 6.48 GPa | 940 ksi | |
Asahi Kasei Xyron® G703V Modified Polyphenylene Ether Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P.. |
|||
Flexural Modulus | 6.48 GPa | 940 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC (Asia Pacific) LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |