Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.47 GPa | 938 ksi | ASTM D790 |
LATI LAPEX A G/20 20% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Flexural Modulus | 6.47 GPa | 938 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP EFL24P PEI LNP* LUBRICOMP* EFL24P is a compound based on Polyetherimide resin containing 20% Glass Fiber, 10% PTFE. Added features of this grade include: Wear Resistant, Exceptional Processing. |
|||
Flexural Modulus | 6.47 GPa | 939 ksi | ASTM D790 |
Samyang Tramid® 210G25 Polyamide, Reinforced Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G25 is a reinforced grade.Applications:Automotive gear level housingConnectors.. |
|||
Flexural Modulus | 6.47 GPa | 939 ksi | ASTM D790 |
Samyang Tramid® 215 Polyamide, High Impact Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.215 is a high impact grade.Applications:Automotive knob types, door handles and m.. |
|||
Flexural Modulus | 6.47 GPa | 938 ksi | ASTM D790 |
SABIC Innovative Plastics ULTEM JD4901 PEI (Asia Pacific) |
|||
Flexural Modulus | 6.47 GPa | 939 ksi | ASTM D790 |
PlastxWorld CEVIAN® B5524 20% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 6.47 GPa | 939 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 60G4 Nylon 66, 20% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |