Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.37 GPa @Thickness 3.20 mm |
925 ksi @Thickness 0.126 in |
ASTM D790 |
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE NSF Certified for KA02 and E2035. Noted for High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts with water co.. |
|||
Flexural Modulus | 6.37 GPa | 925 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN135HB30HI Multi Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 6.37 GPa @Thickness 3.20 mm |
925 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® HI2303 PBT+GF30% Description: Injection Molding, PBT+GF30%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 9003-01-04, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 6.37 GPa | 924 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing 20% Glass Fiber, Proprietary Lubricant. Added features include: Flame Retardant. |
|||
Flexural Modulus | 6.37 GPa | 924 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC (Asia Pacific) LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant, Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 6.37 GPa | 924 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL FM3020V PPE+PS (Asia Pacific) 30% filled FR high modulus foam grade |
|||
Flexural Modulus | 6.37 GPa | 925 ksi | DIN 53452; ASTM D790 |
Kolon SPESIN® KP213G15 Flame Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Flexural Modulus | 6.37 GPa | 925 ksi | DIN 53452; ASTM D790 |
Kolon SPELLOY® KB133G30 PC + PBT Alloy Resin
(discontinued **) SPELLOY® is a new technology of thermoplastic Polymer alloys developed to provide unique combination of excellent mechanical properties.High impact resistance (at low temperature), good dimensional.. |
|||
Flexural Modulus | 6.37 GPa | 925 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN3321G15VO G/F Reinforced & Flame Retardant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstanding .. |