Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Niche Polymer PA66GM40BK Nylon 66, 40% Mineral Fiber Filled Information provided by Niche Polymer |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1033HL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Quadrant EPP Duratron® PAI T5530 Compression Molded Glass Reinforced Polyamide-imide (ASTM Product Data Sheet) |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF18 FR BK 18% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 18% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF20 TL10 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: PTFE Lubricant (10%)Features: LubricatedAppearance: Natural ColorInformation p.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES HiFill® PP 0475 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES Plaslube® J-1/20/TF/20 BK PA66 |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES Plaslube® J-50/20/TF/15 Polycarbonate, 20% Glass Reinforced, PTFE Lubricated 20% Glass Reinforced, PTFE Lubricated |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES Plastiblend® PC/ABS FR GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES Plastiblend® PC/PBT GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES HiFill® ABS GF20 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackTPCI# 9822121Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES HiFill® ABS GF20 LE 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 6.21 GPa | 901 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF0049P PC (Asia Pacific) LNP* Thermocomp* DF0049P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES HiFill® TPX-HTN-03002 A 30% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 30% Filler by WeightFeatures: Platable and High Temperature StrengthUL File Number: E157318Information provided by TP C.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Chase Plastics CP Pryme® N120GL (DAM) Nylon 6, 20% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Westlake Plastics Tempalux® 20% GF Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
Flexural Modulus | 6.21 GPa @Temperature 22.8 °C |
900 ksi @Temperature 73.0 °F |
ASTM D790 |
Ensinger TECAPEI® 20% Glass Reinforced, made from Ultem® 2200 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Flexural Modulus | 6.21 GPa | 901 ksi | ISO 178 |
Azdel Plus C467-B01 45% Chopped Fiber Mat / PP Resin Matrix (Mineral filled) AZDEL® C467-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat and mineral filler contained within a polypropylene resin matrix. This composite material featu.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | Crosswise; ASTM D790 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
PolyOne Edgetek® PI-10CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedElectrically ConductiveInformation provided by PolyOne Corporation. |