Mechanical Properties Metric English Comments
Flexural Modulus 6.13 GPa
889 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RX05495 PA 66
LNP LUBRICOMP* RX05495 is a compound based on Nylon 66 resin containing Glass Bead, Graphite, Glass Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 6.13 GPa
889 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DE002ER PC
LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive.
Flexural Modulus 6.13 GPa
889 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DE002ER PC (Asia Pacific)
LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 6.13 GPa
889 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP JF004LZ PES
LNP* Thermocomp* JF004LZ is a compound based on PES containing 20% Glass Fiber. Added features include: Extrusion Grade, Low Extractible.
Flexural Modulus 6.13 GPa
889 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PF005S PA 6
LNP* THERMOCOMP* PF005S is a compound based on Nylon 6 resin containing 25% Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Modulus 6.13 GPa
889 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PF005S PA 6 (Asia Pacific)
LNP* Thermocomp* PF005S is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Modulus 6.13 GPa
889 ksi
ISO 178
Polyplastics Duranex® 7195W Polybutylene Terephthalate (PBT), Super low warpage, GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 6.13 GPa

@Temperature 65.0 °C
889 ksi

@Temperature 149 °F
ASTM Test
BASF Petra® 130 30% Glass Filled PET