Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.98 GPa | 867 ksi | ASTM D790 |
Omni Plastics OmniTuff™ HPP GRC30 Homopolymer Polypropylene Glass Reinforced Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Flexural Modulus | 5.98 GPa | 867 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6 PA6 GR20 NA Glass Reinforced Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Flexural Modulus | 5.98 GPa @Thickness 6.40 mm |
868 ksi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP2151AF PA6+GF15%, Flame Retardant Feature: Injection Molding, PA6+GF15%, Flame RetardantApplication: ConnectorsCAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Flexural Modulus | 5.98 GPa | 868 ksi | 5 mm/min; ISO 178 |
Gromax BTG30-FN03N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 5.98 GPa | 868 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GR-4020 ABS, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.98 GPa | 868 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GR-4020 ABS, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.98 GPa | 868 ksi | ASTM D790 |
PlastxWorld CEVIAN® EG106 ABS Inherently Static Dissipative and Glass Fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plastx.. |
|||
Flexural Modulus | 5.98 GPa | 867 ksi | ASTM D 790 |
SABIC Innovative Plastics Valox® VC108 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 5.98 GPa | 867 ksi | ASTM D790 |
SABIC Innovative Plastics Lexan® LC108 PC (Asia Pacific) Polycarbonate base, 8% carbon fiber reinforced, FR |
|||
Flexural Modulus | 5.98 GPa | 867 ksi | ASTM D790 |
PlastxWorld CEVIAN® S5220 20% GF PC/ABS alloy Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld .. |