Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.86 GPa | 850 ksi | Tangent; ASTM D790 |
RheTech Products F40-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Battery traysAir cleaner housingFunctional support decksInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific) LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli.. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Polymer Resources NY6-M40-[color]-H Nylon 6, 40% Mineral Filled, Heat Stabilized Nylon 6, 40% Mineral Filled, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Quadrant EPP Duratron® PEI U2300 Extruded 30% Glass Reinforced Polyetherimide (ASTM Product Data Sheet) |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
PolyOne Edgetek® AS-20CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
PolyOne Lubri-Tech™ NL-15CF-15GF/5M Nylon 6/12, Carbon/Glass Filled
(discontinued **) Description/Features:Carbon Fiber ReinforcedGlass Fiber ReinforcedMolybdenum Disulfide LubricatedInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | Tangent; ASTM D790 |
Fiberfil® J-61/30/FR Polypropylene Copolymer, 30% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Techmer ES Electrafil® M-2426 BK Polycarbonate |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 771 PBT 35% mineral/glass reinforced flame retardant grade with a CTI performance level class of 0 rating. Applications which may see electrical arcing. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Techmer ES HiFill® PET 0268 B1 Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Techmer ES HiFill® PP CO GF30 CC 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Techmer ES HiFill® PC GF20 X 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Mold ReleaseFeatures: Good Mold Release and High FlowInformation provided by T.. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Chase Plastics CP Pryme® N320GL (DAM) Nylon 6 (Utility Grade), 20% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Ecomass® 1080ZD94 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided by Techn.. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Ensinger Tecapeek® XP-90 Compression Molded PEEK Compound, 25% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Ensinger Tecatron® XP-84 Compression Molded PPS Compound, 30% Graphite Filled Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
PolyOne Edgetek® ES-20GF/000 Polyethersulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6 GF20 FR HS L 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Adell ER-17 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |