Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.70 GPa | 827 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PC 69 GF 35 FRT 4 Polypropylene Copolymer, 35% Glass Fiber, Halogen Free and Phosphor Free Flame Retardant FeaturesModified copolymer PP for injection moulding, chemically reinforced with 35% glass fiber, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. I.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | |
Plastcom SLOVAMID 66 GF 25 FRI 3 TS PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178, ASTM D790 |
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66 Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char.. |
|||
Flexural Modulus | 5.70 GPa @Temperature 60.0 °C |
827 ksi @Temperature 140 °F |
ASTM D790 |
LATI LARIL 13 G/20-V1 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 15 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced PA 6, 15% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 20 FN20 DUS013 000000 Nylon 6, 20% Glass Fiber PA 6, 20% glass fibers, injection molding, halogen-free flame retardantInformation provided by LANXESS. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PX7446 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP WFL33 PBT LNP* LUBRICOMP* WFL33 is a compound based on PBT containing 15% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East) VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS LNP* STAT-LOY* AF306 is a compound based on ABS resin containing 30% Glass Fiber. Added feature of this material is: Antistatic. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF004 PC (Europe-Africa-Middle East) LNP* THERMOCOMP* DF004 is a compound based on Polycarbonate resin containing Glass Fiber. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Wellman Wellamid® MR409 22H-N 40% Mineral Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178-93 |
Wellman Wellamid® MR409 22H-NBK1 Nylon 66, 40% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM D790 |
Unitika UG-100-30 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM-D790 |
Polyram RamLloy PA917G6 PP/NYLON 66 alloy, 30% Glass Fiber 30% glass fiber reinforced PA66/PP alloy with reduced water absorption, dimensional stability and UV stabilized for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Polyram RamOfin PPH301G6NT Polypropylene, 30% Glass Fiber 30% Glass fiber reinforced polypropylene for injection molding applications. Approved and listed by WRAS Potable Water.Information provided by Polyram. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T BK261 is a 30% glass fiber reinforced toughened black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN 51G15HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G15HSL NC010 is a 15% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | cond.; ISO 178 |
Azoty Tarnow™ Tarnamid® T-27 GF30 I Polyamide 6 - Glass Fiber Reinforced 30% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 413 Glass Reinforced, Polycarbonate/Polyester Alloy, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |