Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.65 GPa | 820 ksi | Tangent; ASTM D790 |
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black Applications: Electrical component housingsSunroof componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 5.65 GPa | 820 ksi | ASTM D790 |
Quadrant EPP Techtron® PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded (ASTM Product Data Sheet) |
|||
Flexural Modulus | 5.65 GPa | 819 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY DF2049 PC (Asia Pacific) LNP* Lubriloy* DF2049 is a compound based on Polycarbonate resin containing Glass Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Flame Retardant. |
|||
Flexural Modulus | 5.65 GPa | 820 ksi | ASTM D790 |
Techmer ES Electrablend® PC SS15 FR BK 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation pr.. |
|||
Flexural Modulus | 5.65 GPa | 820 ksi | ASTM D790 |
Techmer ES HiFill® ABS GF20 IM 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedTPCI# 7782121Information provided by T.. |
|||
Flexural Modulus | 5.65 GPa | 820 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 CM40 6122 BK 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackProcessing Method: Injection Mol.. |
|||
Flexural Modulus | 5.65 GPa | 820 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF/B40 L 20% Glass Bead/Glass Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by Weight and Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation .. |
|||
Flexural Modulus | 5.65 GPa | 819 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX06411 PC LNP* THERMOCOMP* DX06411 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare. |
|||
Flexural Modulus | 5.65 GPa | 819 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX06411 PC (Asia Pacific) LNP* Thermocomp* DX06411 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Flexural Modulus | 5.65 GPa | 819 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp JF003L PES LNP* Thermocomp* JF003L is a compound based on Polyethersulfone (PES) containing Glass Fiber. Characteristics of this grade are Low Extractable.This data was supplied by SABIC-IP for the Americas r.. |
|||
Flexural Modulus | 5.65 GPa | 820 ksi | ASTM D790 |
Techmer ES HiFill® PA6 0201 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.65 GPa | 820 ksi | ASTM D790 |
PlastxWorld CEVIAN® A2606 30% GF PA/ABS Alloy, Conditioned Property data is for samples at equilibrium moisture (0.7%)These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWo.. |
|||
Flexural Modulus | 5.65 GPa | 819 ksi | ISO 178 |
Polyplastics Duranex® C5315 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 5.65 GPa | 820 ksi | ASTM D790 |
Asahi Kasei Thermylene® P7-30FG-0874 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 5.65 GPa | 820 ksi | ASTM D790 |
Solvay Specialty Polymers Supradel® HTS-2620 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2620 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance .. |