Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Polymer Resources NY6-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | Tangent; ASTM D790 |
Fiberfil® J-60/20/FR Polypropylene Homopolymer, 20% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® PCGF120 Polycarbonate, 20% Glass-Filled 20% glass-filled grade, good balance of impact and mechanical propertiesAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 5.52 GPa | 801 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® XE5515BL Polyphenylene Sulfide Alloy (PPS Alloy), 15% Glass Fiber Ryton® XE5515BL 15% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength and chemical resistance at elevated temperatures and is suitable for extrusi.. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF20 HS L 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedInformati.. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF20 L 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES HiFill® PP GF/M40 CC BK 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES HiFill® PP GF/M50 CC BK 50% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.52 GPa | 801 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX4605 PPE+PS PPE+PS blend. 20% Glass reinforced. High heat. Dimensional stability. Suitable for automotive and E/E applications. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES HiFill® PES GM20 WT139 20% Milled Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN113L (Dry) Nylon 66, 13% Glass Fiber Reinforced, Lubricated Features: Good chemical resistanceGrease resistantLubricatedOil resistantHigh rigiditySolvent resistantHigh tensile strengthForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | Crosswise; ASTM D790 |
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | Crosswise; ASTM D790 |
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Aaron Industries AAROPRENE® GFN 6013 Glass Filled Nylon 6 AAROPRENE® GFN &G/MFN 6000 Series Reinforced CompoundsColor may be specified. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Aaron Industries AAROPRENE® GFPP 2040 Glass Filled Polypropylene AAROPRENE® GFPP 2000 Series Glass Reinforced CompoundsMelt flow index may be specified. Color may be specified. |