Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC (Asia Pacific) LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing 15% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KFL32R Acetal Copolymer LNP LUBRICOMP* KFL32R is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE. Added feature of this material is: Easy Release, Wear Resistant. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP MX06404 PP (Asia Pacific) LNP* LUBRICOMP* MX06404 is a compound based on Polypropylene resin containing PTFE, Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 (Asia Pacific) LNP* Lubricomp* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 855 PBT 15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 855 PBT (Asia Pacific) 15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® DR51 PBT 15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® DR51 PBT (Asia Pacific) 15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® DR51M PBT (Asia Pacific) 15% GR; exc. mechanical/thermal/electrical performance; nonflame retardant. For spotlights, appliance housings, handles. Easy flow/int. mold release.This data was supplied by SABIC-IP for the Asia .. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® K4530 PBT (Europe-Africa-Middle East) 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp EB004 PEI LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp EB004 PEI (Asia Pacific) LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12 LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12 (Asia Pacific) LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly LNP* THERMOCOMP* KF002L is a compound based on Acetal Homopolymer resin containing 10% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly (Asia Pacific) LNP* Thermocomp* KF002L is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 5201-12 Polycarbonate Resin Overview: CALIBREâ„¢ 5201-12 polycarbonate resin is 20% glass reinforced containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. CALI.. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | 3-point; ISO 178 |
Styron CALIBREâ„¢ 5201-8 Polycarbonate Resin Overview: CALIBREâ„¢ 5201-8 polycarbonate resin is 20% glass reinforced containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. CALIB.. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D790 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D790 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D790 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D790 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D790 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | ASTM D790 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.82 GPa | 699 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® K4530 PBT 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |