Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.68 GPa | 679 ksi | ISO 178 |
FKuR Kunststoff Bio-Flex® S 9533 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Flexural Modulus | 4.68 GPa | 679 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developed for automotive bezel application that requires basecoat + .. |
|||
Flexural Modulus | 4.68 GPa | 679 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific) Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +.. |
|||
Flexural Modulus | 4.68 GPa | 679 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DF0029P PC LNP THERMOCOMP* DF0029P is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant. |
|||
Flexural Modulus | 4.68 GPa | 679 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP JF002 PES (Asia Pacific) LNP THERMOCOMP* JF002 is a compound based on Polyethersulfone resin containing Glass Fiber. |
|||
Flexural Modulus | 4.68 GPa | 679 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp JX89569 PES LNP THERMOCOMP* JX89569 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 4.68 GPa | 679 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp JX89569 PES (Asia Pacific) LNP* THERMOCOMP* JX89569 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |