Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.414 GPa | 640.2 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylex® P1310G15 HB Polycarbonate, 15% Fiberglass Reinforced, UV Stabilized Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Entec. |
|||
Flexural Modulus | 4.414 GPa | 640.2 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylex® P1010G15 HB Polycarbonate, 15% Fiberglass Reinforced Information provided by Ravago. |