Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.27 GPa | 620 ksi | Resin |
Renegade Materials Corporation RM-3000 Bismaleimide (BMI) 6781 S2 Glass Fabric Developed using state-of-the-art formulating technologies, RM-3000 One Part BMI RTM Resin delivers superior hot/wet performance in airframe, missile and
propulsion applications at service temperatu.. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | Resin |
Renegade Materials Corporation RM-3000 Bismaleimide (BMI) Resin Developed using state-of-the-art formulating technologies, RM-3000 One Part BMI RTM Resin delivers superior hot/wet performance in airframe, missile and
propulsion applications at service temperatu.. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | Resin |
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures .. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | Resin |
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin 4581 Astroquartz III Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures .. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | Resin |
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin IM7 12K Carbon Uni-tape Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures .. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | Resin |
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin T650-35-6K-UC309-5HS Carbon Fabric Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures .. |
|||
Flexural Modulus | 4.27 GPa | 619 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp DFL329EF PC LNP LUBRICOMP* DFL329EF is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant.This data was supplied by .. |
|||
Flexural Modulus | 4.27 GPa @Temperature 23.0 °C |
619 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th.. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | Tangent; ASTM D790 |
Fiberfil® J-69/20/E High performance polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | ASTM D790 |
Techmer ES Electrablend® ABS CF5 5% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 5% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.27 GPa @Temperature 23.0 °C |
619 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GB25 L BK 25% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 25% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | ASTM D790 |
Techmer ES Luriblend® POM CO GF10 TL10 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionApp.. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN133GTL (COND, 50% RH) Nylon 66, 33% Glass Fiber Reinforced, Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | Tangent; ASTM D790 |
Washington Penn Medium Impact Copolymer 50% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® GFPP-30 30% Glass-Reinforced Polypropylene Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuou.. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | ASTM D790 |
Ensinger Tecapeek® XP-101 Compression Molded PEEK Compound, Filled with 15% Graphite and 10% PTFE Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Modulus | 4.27 GPa | 619 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFL329 PC LNP LUBRICOMP* DFL329 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | ASTM D790 |
PlastxWorld CEVIAN® A2603 15% GF PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 4.27 GPa | 620 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® NY1GF130 Nylon 6, 13% Glass-Filled 13% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |