Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178 |
Nilit FRIANYL A63 CU90 Nylon 6.6 for injection molding, 90% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178 |
Nilit FRIANYL A63 GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 4.20 GPa @Temperature 23.0 °C |
609 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANAMID 66 A32^E Q30 Nylon 66, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 4.20 GPa @Temperature 23.0 °C |
609 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANAMID 66 A43^E F14 Nylon 66, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Modulus | 4.20 GPa @Temperature 23.0 °C |
609 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANMID 6 B32^ E Q30 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Modulus | 4.20 GPa @Temperature 23.0 °C |
609 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANMID 6 B43^ D F15 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | |
Plastcom SLOVAMID 6 GF 15 MI/2 PA6, 15% glass fibre, improved strength FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178 |
Victrex® HT™ P45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion
compounding, low flow, FDA food contact compliant, co.. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | |
Lehmann & Voss LUVOCOM® 1105-8127 PEEK, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 2mm/min; ASTM D790 |
Kingfa JH710 G10 Flame Retardant & 10% Glass Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 1-2140 BLH 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-2140 BLH is recommended especially for producing products, where high stiffness, low shrinkage, long term heat stability and excellent processability are required.All information pr.. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 1-6140 N 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-6140 N is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-6140 N is developed for producing injection molded components for household eq.. |
|||
Flexural Modulus | 4.20 GPa @Temperature 80.0 °C |
609 ksi @Temperature 176 °F |
2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC STAMAX 30YM240 PP SABIC® STAMAX 30YM240 is a 30% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16496906... |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Asia Pacific) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP NF002 PC+ABS LNP THERMOCOMP* NF002 is a compound based on PC+ABS resin containing 10% Glass Fiber. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178-93 |
Wellman Wellamid® FRGS25-66-NBK3 Nylon 66, 25% Glass Sphere Reinforced, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178 |
Polyram PlusTek PB826G3 Nylon 6 for Injection Molding, 15% Glass-fiber Reinforced, Impact Modified and UV Stabilized 15% Glass fiber reinforced, impact modified and UV stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | cond; ISO 178 |
DSM Novamid® 1010GN2-15Z BK701 PA6-GF15 FR(17) 15% Glass Reinforced, Flame Retardant, Easy Molding Grade, Injection Molding, High Flow |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide PF003IX1 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF003IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF1003HI005)Information provided by Eurostar. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 2 mm/min; ISO 178 |
Eurostar Starglas GX05052 PSU, Glass Fiber Filled Starglas GX05052 is a Glass Fiber Reinforced PSU resin (also known as Starglas PSU A 10V ¾)Information provided by Eurostar. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 2 mm/min; ISO 178 |
Eurostar Starpylen MFB44S PP, Glass Bead/Glass Fiber Filled Starpylen MFB44S is a Glass Beads, Glass Fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WS 2020VK S37.7)Information provided by Eurostar. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO Data |
BASF Ultradur B 4300 G2 BK5110 10% Glass Filled PBT Ultradur B 4300 G2 BK5110 is a pigmented black, easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO Data |
BASF Ultramid® NFX-0102 NF2004 30% Glass Filled PA66 (Dry) Ultramid NFX-0102 NF2004 is a heat stabilized, 30% glass bead PA66 injection molding grade. It is especially formulated for low warp, increased stiffness and excellent dimensional stability. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® VX4015 PBT (Europe-Africa-Middle East) VALOX VX4015 is a 15% glass reinforced PBT injection moulding resin, with excellent hydrolytical stability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178 |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178 |
BASF Ultramid® B3WG5 BK 00564 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |