Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.17 GPa | 605 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32 PC LNP LUBRICOMP* DFL32 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 4.17 GPa | 605 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32XXC PC LNP LUBRICOMP* DFL32XXC is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 4.17 GPa | 604 ksi | ASTM D790 |
UBE UPIMOL® R Polyimide Shape Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub.. |