Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Oxford Polymers Oxnilon 66-13GF 13% Glass Fiber Filled Nylon 66 for Injection Molding 13% Glass Fiber Filled Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet) |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Polymer Resources PC-G15 Polycarbonate, 15% Glass Reinforced Polycarbonate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polym.. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Technetics Group Amicon™ PEEK
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Quadrant EPP Semitron® CMP XL20 (ASTM Product Data Sheet) |
|||
Flexural Modulus | 4.14 - 30.1 GPa | 600 - 4360 ksi | Average value: 11.4 GPa Grade Count:26 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF/M25 HS L BK 25% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackTPCI.. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Techmer ES HiFill® PP GF20 CC HS 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and Chemically CoupledInformation pro.. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Techmer ES Statiblend® ABS GF15 AS 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Techmer ES HiFill FR® PP GF10 FR BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightFeatures: Flame Retardant Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
PolyOne Edgetek® ES-10GF/000 PES (Polyethersulfone), 10% Glass Reinforced, Hi-Temp
(discontinued **) Information provided by PolyOne™ Corporation |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
PolyOne Edgetek® PE-30GF/000 WHITE High Density Polyethylene (HDPE), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedWhitePolyOne First ChoiceInformation provided by PolyOne Corporation. |