Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 31.034 GPa | 4501.1 ksi | ASTM D-790 |
PlastiComp Complet® LCF40-PEI Polyetherimide, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyetherimide with 40% long carbon fiber reinforcementInformation provided by PlastiC.. |