Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 30.2 GPa | 4380 ksi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
(Unverified Data**) AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot.. |
|||
Flexural Modulus | 30.2 GPa | 4380 ksi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK) AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th.. |