Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.87 GPa | 561 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OL003A PPS - Branched LNP* LUBRICOMP* OL003A is a compound based on PPS - Branched resin containing 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
Flexural Modulus | 3.87 GPa | 561 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RB004 PA 66 LNP* THERMOCOMP* RB004 is a compound based on Nylon 66 containing Glass Beads. |
|||
Flexural Modulus | 3.87 GPa | 561 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.87 GPa | 561 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.87 GPa | 561 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.87 GPa | 561 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.87 GPa | 561 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.87 GPa | 561 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.87 GPa | 561 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.87 GPa | 561 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.87 GPa | 561 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.87 GPa | 561 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.87 GPa | 561 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.87 GPa | 561 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.87 GPa | 561 ksi | ASTM D790 |
Entec Hyril® GP355AS Styrene Acrylonitrile Available in North America Features: Copolymer Automotive Specifications: DELPHI M-9565-9 Color: Blue-TransparentForm: PelletsProcessing Method: ExtrusionInformation provided by Entec |
|||
Flexural Modulus | 3.87 GPa | 561 ksi | ASTM D790 |
Entec Hyril® SAN500 Styrene Acrylonitrile Available in North America Features: Copolymer Form: PelletsInformation provided by Entec |