Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.82 GPa | 554 ksi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics Lexan® FL410 PC Various weight reductions at 0.250: (6.38 mm) wall. Thin wall capability high flexural mod, strength and creep resistant. V-0/5V - 0.157""(3.98 mm). |
|||
Flexural Modulus | 3.82 GPa @Thickness 3.20 mm |
555 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® HI2100M PBT+GF10% Description: Injection Molding, PBT+GF10%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 65997-17-3, 155123-66-3 and 30965-26-5Information provided by LG Chemical |
|||
Flexural Modulus | 3.82 GPa @Thickness 6.40 mm |
555 ksi @Thickness 0.252 in |
5mm/min; ASTM D790 |
LG Chemical Lupox® TE5100 PBT+PC+GF10% Description: Injection Molding, PBT+PC+GF10%, High Impact resistant, Dimensional StabilityApplication: Automotive (Bumper Back Beam)CAS No. 30965-26-5, 103598-77-2 and 65997-17-3Information provided.. |
|||
Flexural Modulus | 3.82 GPa | 554 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL INT1512 PPE+HIPS (Asia Pacific) PPE/HIPS GF filled for auto interior |