Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.80 GPa | 551 ksi | ISO 178, ASTM D790 |
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66 Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app.. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | ISO 178 |
Nilit FRIANYL A63 H-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | ISO 178 |
Nilit FRIANYL A63 W-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 3.80 GPa @Temperature 23.0 °C |
551 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANAMID 66 A11^ X30 Nylon 66, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.80 GPa @Temperature 23.0 °C |
551 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANAMID 66 A12^ X30 Nylon 66, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | |
Plastcom SLOVASTER® B1 HML GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist.. |
|||
Flexural Modulus | 3.80 GPa @Temperature 23.0 °C |
551 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH T1040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.80 GPa @Temperature 23.0 °C |
551 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH T2040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.80 GPa @Temperature 23.0 °C |
551 ksi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 450P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, standard flow, FDA food contact comp.. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | ISO 527 |
Victrex® PEEK 450PF Fine Powder Grade Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, standard flow, FDA food contact complia.. |
|||
Flexural Modulus | 3.80 - 4.20 GPa | 551 - 609 ksi | ASTM D790 |
Loxim 830 12 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | ISO 178 |
Lanxess Durethan® BKV 215 H3.0 000000 Nylon 6-Copolymer, 15% Glass Fibers PA 6-Copolymer, 15% glass fibers, injection molding, impact modified |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK) KetaSpire® KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry.. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East) VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ER PC (Europe-Africa-Middle East) LNP* THERMOCOMP* DF002ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features include Easy Molding, Mold Release. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | 2mm/min; ISO 178 |
Teijin Multilon DN-3510F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 10 % filler. Improved stiffness and high fluidity realizes a thin wall.. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | ASTM D 790 |
Saint-Gobain Meldin® 2211 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Ser.. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Asia Pacific) NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | ISO 178-93 |
Wellman Wellamid® GB1430-N 33% Glass Bubble Filled, Low Density Nylon 66 Description: Glass Bubble Filled, Low Density Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | ISO 178 |
Wellman Wellamid® GFT13-66 XE-N 13% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | ASTM D 790 |
Cossa Polimeri ESTAPROP HK 1280 T8 Polypropylene, 40% Mineral Filled PP homopolymer 40% mineral fillerExcellent physical and mechanical characteristics, good surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | ASTM D790 |
Diamond Polymers NPP30-0500 GF20 20% Glass Filled Black Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | ASTM D790 |
Adell AJ-33 Nylon 66, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 3.80 GPa @Temperature 23.0 °C |
551 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH T5040 FC Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.80 GPa @Temperature 23.0 °C |
551 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH T5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.80 GPa | 551 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX2391 PPE+HIPS (Europe-Africa-Middle East) PX2391 is a 10% glass fiber reinforced, heat stabilized, low odor and low emission NORYL(R) grade for interior automotive applications, especially instrument panels |