Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.64 GPa | 528 ksi | ASTM D790 |
NOVA Chemicals Dylark® 232 High Performance Styrenic, Transparent Grade High heat resistance, Sparking water-white clarity, Good chemical resistance, High modulus, for superior shear and torque resistanceApplications: Light pipes and lighting, High heat microwave packag.. |
|||
Flexural Modulus | 3.64 GPa | 528 ksi | ASTM D 790 |
NOVA Chemicals Dylark® FG7200 High-Heat Styrenic Copolymer Product Description and Features: Styrene/maleic anhydride copolymer with high-heat resistance and high modulus. Resins designed for use in foam extrusion.Processing: Contact NOVA Chemicals techn.. |
|||
Flexural Modulus | 3.64 GPa | 528 ksi | ISO 178 |
Polyplastic Armlen® PP GF MF 30-1 Polypropylene, 30% Glass and Mineral Filled Injection moldingInformation provided by PolyPlastic Group. |
|||
Flexural Modulus | 3.64 GPa | 528 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL EM7301F PPE+PS 10% glass-reinforced. HDT 252F. Good flow and polyurethane foam adhesion. Black only. |