Mechanical Properties Metric English Comments
Flexural Modulus 3.35 GPa
486 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion L7703 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Flexural Modulus 3.35 GPa
486 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CM5820 PC+ABS (Asia Pacific)
Cycoloy CM5820 resin is a Mineral Filled Non-FR PC+ABS blend with high impact, high modulus, good chemical resistance & improved surface aesthetic, designed for hand help device chassis that require..
Flexural Modulus 3.35 GPa
486 ksi
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Flexural Modulus 3.35 GPa
486 ksi
ASTM D790
Solvay TECHNYL® A 205F PA66, DRY
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Flexural Modulus 3.35 GPa
486 ksi
ASTM D790M
DSM Somos® ProtoTherm™ 12110 Water-resistant resin for stereolithography, UV Postcure
DescriptionDSM Somos® 12110 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12110 have a cherry-red appearance which tur..
Flexural Modulus 3.35 GPa
486 ksi
2mm/min; ISO 178
Denka TX-600S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Flexural Modulus 3.35 GPa
486 ksi
2mm/min; ASTM D790
Denka TX-100S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene