Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.068 GPa
445.0 ksi
ASTM D790
Ineos Nova 2580 General Purpose Crystal Polystyrene  (discontinued **)
High speed molding, Improved crack resistanceApplications: Cutlery, Consumer electronicsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optic..
Flexural Modulus 3.068 GPa
445.0 ksi
ASTM D790
Ineos Nova 2510 General Purpose Crystal Polystyrene  (discontinued **)
High speed molding, Improved crack resistance, USP Class VIApplications: Cutlery, Light louvers, RazorsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phy..
Flexural Modulus 3.068 GPa
445.0 ksi
ASTM D790
Ineos Nova 2511 General Purpose Crystal Polystyrene  (discontinued **)
High speed molding, Improved crack resistance, USP Class VIApplications: Cutlery, Light louvers, RazorsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phy..
Flexural Modulus 3.068 GPa
445.0 ksi
ASTM D790
Ineos Nova 2581 General Purpose Crystal Polystyrene  (discontinued **)
Good blending resin, Good balance of flow, strength and heat resistanceApplications: Consumer electronics, HousewaresExposure to gamma radiation in the 2.02-6.06 megarad range has no significant eff..