Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.037 GPa | 440.5 ksi | ASTM D790 |
Ineos Nova 1511 High Heat Crystal Polystyrene
(discontinued **) High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical.. |
|||
Flexural Modulus | 3.037 GPa | 440.5 ksi | ASTM D790 |
Ineos Nova 2100 General Purpose Crystal Polystyrene
(discontinued **) Relative high heat resistance, Improved crack resistance, Good strengthApplications: Foam extrusion, Biaxially oriented sheet, Thermoforming applications, Molded packagingExposure to gamma radiation.. |
|||
Flexural Modulus | 3.037 GPa | 440.5 ksi | ASTM D790 |
Ineos Nova 3601 General Purpose Crystal Polystyrene
(discontinued **) Easy flow for high productivity, excellent post molding scuff resistanceApplications: Medical, LabwareExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phys.. |
|||
Flexural Modulus | 3.037 GPa | 440.5 ksi | ASTM D790 |
Ineos Nova 1300 High Heat Crystal Polystyrene High heat resistance, High strength, Good processing characteristics, USP Class ViApplications: Electronics packaging, Medical packaging, Cosmetic cases, Profile extrusionExposure to gamma radiation.. |
|||
Flexural Modulus | 3.037 GPa | 440.5 ksi | ASTM D790 |
Ineos Nova 1510 High Heat Crystal Polystyrene High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical.. |
|||
Flexural Modulus | 3.037 GPa | 440.5 ksi | ASTM D790 |
Ineos Nova 1301 High Heat Crystal Polystyrene High heat resistance, High strength, Good processing characteristics, USP Class VIApplications: Electronics packaging, Medical packaging, Cosmetic cases, Profile extrusionExposure to gamma radiation.. |