Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.0030 GPa | 435.55 ksi | ASTM D790 |
Westlake Plastics HTP 800 Clear PVC HTP 800 is a clear PVC based material for use as windows and doors in cleanroom equipment. Notable properties include light transmission, chemical resistance, and flame resistance. Information prov.. |