Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 25.5 GPa @Temperature 23.9 °C |
3700 ksi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® P-670F Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-670F is a versatile, non-styrenated/low VOC polyester resin. P670F is used in a wide variety of applications including tooling and aircraft structures.Key Features and Benefits:Non-styre.. |
|||
Flexural Modulus | 25.5 GPa | 3700 ksi | ASTM D790 |
LNP Stat-Kon® EC-1008 EM BK8-115 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically Conductive, Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev.. |
|||
Flexural Modulus | 25.5 GPa | 3700 ksi | ASTM D790 |
Greene Tweed Orthetek® RP Polyketone, Random Carbon Fiber Greene Tweed offers precision-molded thermoplastic components made form out high-performance Orthtek® composite materials for a variety of demanding medical device applications. Orthtek RP is id.. |