Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 22.75 GPa | 3300 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP UCF26AS PPA LNP* THERMOCOMP* UCF26AS is a compound based on Polyphthalamide resin containing 30% Carbon Fiber, 10% Glass Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive.. |
|||
Flexural Modulus | 22.75 GPa | 3300 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP UCF26AS PPA (Asia Pacific) LNP* Thermocomp* UCF26AS is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Heat Stabilized. |