Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 21.5 GPa | 3120 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert.. |
|||
Flexural Modulus | 21.5 GPa | 3120 ksi | ISO 178 |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Flexural Modulus | 21.5 GPa | 3120 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical.. |
|||
Flexural Modulus | 21.5 GPa | 3120 ksi | longitudinal; ISO 178 |
Bond Laminates TEPEX® dynalite 108-FGAL290(1)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea.. |
|||
Flexural Modulus | 21.5 GPa | 3120 ksi | longitudinal; ISO 178 |
Bond Laminates TEPEX® dynalite 108-FGAL290(2)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea.. |
|||
Flexural Modulus | 21.5 GPa | 3120 ksi | longitudinal; ISO 178 |
Bond Laminates TEPEX® dynalite 108-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea.. |