Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.94 GPa | 426 ksi | ASTM D790 |
PolyOne Geon™ HTX Ultra LA427Plus Polyvinyl Chloride Alloy (PVC Alloy) Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties based on Geon HTX Ultra LA427Plus Natural 0000Information provided by PolyOne |
|||
Flexural Modulus | 2.94 GPa | 427 ksi | ASTM D790 |
Omni Plastics OmniTuff™ HPP TF20 Homopolymer Polypropylene Talc Filled Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Flexural Modulus | 2.94 GPa | 426 ksi | ASTM D790 |
LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic
(Unv Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Flexural Modulus | 2.94 - 3.79 GPa | 426 - 550 ksi | Average value: 3.27 GPa Grade Count:5 |
Overview of materials for Thermoplastic Polyimide, Unfilled |
|||
Flexural Modulus | 2.94 GPa | 426 ksi | ASTM D790 |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Flexural Modulus | 2.94 GPa | 427 ksi | ASTM D790 |
I. Stern GPPS-020 General Purpose Crystal Polystyrene Features:High Strength GradeHigh Flow, High ToughnessExcellent ProcessabilityApplicationsInjection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & Co... |
|||
Flexural Modulus | 2.94 GPa @Thickness 6.40 mm |
427 ksi @Thickness 0.252 in |
15mm/min; ASTM D790 |
LG Chemical LUCON CP6052 PC/ABS+CNT Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, Low Surface Resistivity, Improved Impact StrengthApplication: Laser diode Tray, ATM parts, Telecommunication Station Housi.. |
|||
Flexural Modulus | 2.94 GPa | 427 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN126 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 2.94 GPa @Thickness 3.20 mm |
427 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an.. |
|||
Flexural Modulus | 2.94 GPa | 427 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN136 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 2.94 GPa | 427 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN3311 General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Modulus | 2.94 GPa @Thickness 6.40 mm |
427 ksi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOL HI2202B PP+GF20%, High Impact Description: Injection Molding, PP+GF20%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 65997-17-3 and 9010-79-1Information provided by LG Chemica.. |
|||
Flexural Modulus | 2.94 GPa | 426 ksi | ASTM D790 |
KKPC Kuhmo GP 125EB Extrusion Molding GPPS Key features: PSP Common Uses: Fruit, egg cell.GPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding processability, and stability of dimension.Da.. |
|||
Flexural Modulus | 2.94 GPa | 427 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN132VO Flame Retardant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 2.94 GPa | 427 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN171 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 2.94 GPa | 427 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN3311N General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Modulus | 2.94 GPa | 426 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP LL003 PEEK LNP* LUBRICOMP* LL003 is a compond based on Polyetheretherketone resin containing 15% PTFE Lubricant. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.94 GPa | 426 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp RL001 PA 66 LNP Lubricomp* RL001 is a Nylon 6/6 base resin containing PTFE lubricant. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.94 GPa | 427 ksi | |
Shinil Chemical SHINSTAT MS Electrostatic Control Polymer Injection Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Flexural Modulus | 2.94 GPa | 427 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® CF-3104HF PC, 10% Glass Filled High Impact High-impact PC/GR material for the exterior of slim mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.94 GPa | 427 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® CF-3104HF PC, 10% Glass Filled High Impact High-impact PC/GR material for the exterior of slim mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.94 GPa | 426 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PKN4752 PPE+PS PPE+PS blend. High Heat. Translucent with yellow tint in natural color. FDA compliant. Extrusion and Injection Molding. Typical applications include High Performance Food Packaging, Electronics and .. |
|||
Flexural Modulus | 2.94 GPa | 426 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PKN4752 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High heat. Extrusion. Microwavable. Food, electrical/electronic packaging uses. |
|||
Flexural Modulus | 2.94 GPa | 426 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp LL003E PEEK LNP* Lubricomp* LL003E is a compound based on Polyetheretherketone (PEEK) containing PTFE. Characteristics of this grade are: Easy Molding and Internally Lubricated.This data was supplied by SABIC.. |
|||
Flexural Modulus | 2.94 GPa @Thickness 3.20 mm |
427 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SC 201E General Purpose Polystyrene CharacteristicsVery high molecular weight High heat grade Good melt strength Good clarity and mechanical strengthProcessing Extrusion MoldingApplicationsExtruded embossed sheets, OPS, foamed meat t.. |
|||
Flexural Modulus | 2.94 GPa @Thickness 3.20 mm |
427 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SC 208 General Purpose Polystyrene CharacteristicsHigh flow grade Easy processing Good clarity & shineProcessing Extrusion MoldingApplications Hand molding applications of novelty items, toys etc. Carrier for master batches, as a .. |
|||
Flexural Modulus | 2.94 GPa | 426 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF VF1001S Super Tough Nylon LNP* Thermotuf* VF1001S is a Super Tough Nylon containing glass fiber. Characteristics of this grade is Heat Stabilized. |
|||
Flexural Modulus | 2.94 GPa | 426 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL EXNL0143 PPE+PS Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica.. |
|||
Flexural Modulus | 2.94 GPa | 426 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX1736 PPE+PS Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica.. |
|||
Flexural Modulus | 2.94 GPa @Thickness 3.20 mm |
427 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP201 4551 Light Stabilized Polystyrene Characteristics Excellent light stability to fluorescent & incandescent light sources Very high clarity and heat resistance Excellent strength & stiffness Processing Injection molding Extrusion A.. |