Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.55 GPa | 370 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® EHA PC+ABS PC+ABS. Electroplateable. |
|||
Flexural Modulus | 2.55 GPa @Thickness 3.20 mm |
370 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HG193S ABS, High Flow, Chemical Resistance Feature: Injection Molding, High Flow, Chemical ResistanceApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Modulus | 2.55 GPa @Thickness 3.20 mm |
370 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID GP1300A(W) PA6, High Viscosity Feature: Injection Molding, PA6, High ViscosityApplication: Automotive PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Flexural Modulus | 2.55 GPa @Thickness 3.20 mm |
370 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5001RFT PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Flexural Modulus | 2.55 GPa | 370 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® ACR100IM Polymethylmethacrylate, High Impact High impact version, extrusion or injection molding PMMAAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 2.55 GPa @Thickness 6.40 mm |
370 ksi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HI5302S PP+MF15%, High Impact Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsInformation provided by LG Chemical |
|||
Flexural Modulus | 2.55 GPa @Thickness 3.20 mm |
370 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY ER5001RFA PC/ABS, Halogen Free, Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.55 GPa @Thickness 3.20 mm |
370 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR404 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf.. |
|||
Flexural Modulus | 2.55 GPa | 370 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Flexural Modulus | 2.55 GPa | 370 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1014S PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.55 GPa | 370 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® EA-0640 ABS, Unreinforced Permanent static prevention ABS material such as LCD carrierInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.55 GPa | 370 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® NH-1907 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.55 GPa | 370 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1014S PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.55 GPa | 370 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 2.55 GPa | 370 ksi | ASTM D790 |
PlastxWorld CEVIAN®-V 510 ABS High Modulus ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 2.55 GPa | 370 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN100M2 (Dry) Nylon 66, Lubricated Features: Good chemical resistanceFast cycleDurableLubricatedSolvent resistantInjection moldingForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 2.55 GPa | 370 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN100M2HS (Dry) Nylon 66, Lubricated, Heat Stabilized Features: Good chemical resistanceFast cycleDurableHeat stabilizedLubricatedSolvent resistantInjection moldingForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 2.55 GPa | 370 ksi | ASTM D790 |
Westlake Plastics PES film Made from ULTRASON® E Polyethersulfone Resin High heat deflection and continuous use temperature. Exceptional tensile and flexural strength. High dielectric strength. Exceptional mechanical properties. Dimensionally stable at varying tempera.. |
|||
Flexural Modulus | 2.55 GPa | 370 ksi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® 740V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |