Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.53 GPa | 367 ksi | ASTM D790 |
PolyOne Novablend™ 4578 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | ASTM-D790 |
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM ATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM ATX100 PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem ATX100F PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem ATX100F PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem ATX100R PEI+PCE Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem ATX100R PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | ASTM D790 |
Spartech Millennium III Glass Filled PC Structural Sheet Description: Structural SheetInformation provided by Spartech. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX500 PPE (Asia Pacific) Noryl PX500 is an unfilled modified polyphenylene ether resin capable of multiple conversion routes. This resin is designed for lower odor during conversion than many standard modified PPE resins. .. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP YF005 TPEE (Asia Pacific) LNP* Thermocomp* YF005 is a compound based on TPEE resin containing Glass Fiber. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL FP3060 PPE+PS (Europe-Africa-Middle East) Noryl* FP3060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL N1050 PPE+HIPS (Asia Pacific) Noryl* N1050 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow , this resin also uses non-chlorinated, non-brominated FR ad.. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL N1250 PPE+HIPS (Asia Pacific) Noryl* N1250 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow , this resin also uses non-chlorinated, non-brominated FR ad.. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | ISO 178 |
Polyplastics Duranex® CN7000 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50% DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Flexural Modulus | 2.53 GPa | 367 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |