Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.50 GPa @Temperature 23.0 °C |
363 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PP CIP16020FCS Polypropylene, Fast Cycle Information provided by Polykemi AB |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties for a wide variety of applications including business equipment, TVs, monitors, enclosures, among others.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY XP4034 ASA+PC (Europe-Africa-Middle East) GELOY XP4034 is a high heat modified ASA+PC alloy. It is a weatherable, injection mouldable product which is available in a wide range of colours. The product is recommended for automotive unpainted.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML3042 PC (Europe-Africa-Middle East) LEXAN ML3042 offers an extremely low light transparency in combination with a very high reflection. This product is ideally suited for lighting reflectors. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Asia Pacific) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Flexural Modulus | 2.50 GPa @Temperature 23.0 °C |
363 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYabs F30 ABS Information provided by Polykemi AB |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
Nilit FRIANYL B63 H Nylon 6 for injection molding Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXRL0627 PC Copolymer EXRL0627 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and transparent colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ASTM D790 |
Perstorp Compounds Akestra™ 90 Thermoplastic Copolyester Akestra™ is a thermoplastic with a sparkling glass-like appearance. It can be used as a polystyrene alternative for heat resistant thin wall containers, a polycarbonate alternative for durable “di.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ASTM D790 |
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | |
Lehmann & Voss LUVOCOM® 1-7360/EG Polyamide 66, with PTFE, lubricant modified, high viscosity, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property.Bea.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
Manifattura Cattaneo POM c Acetal Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
Ineos ABS Lustran® ABS 680 LNS503 High Performance Injection Molding Grade Lustran® ABS 680 LNS503 is an easy flow version. It is a high performance injection molding grade used for refrigerator and freezer door end caps. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL RN0401 PPE+PS (Europe-Africa-Middle East) Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KA000 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KA000 is a compound based on Acetal Copolymer resin containing Aramid Fiber, Proprietary Lubricant. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RL004 is a compound based on Nylon 66 resin containing PTFE. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | |
SPS Guang Zhou FILLMAâ„¢ 5002F30C Mineral Filled Polypropylene Characteristic: 30%wt of Sulfate Calcium filled, low odor, good glossApplications: Household appliance parts, office suppliesInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ASTM D790 |
Unitika L-8005 Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide R1000K PA66, Injection Molded Staramide R1000K is an Unreinforced Radiation Crosslinkable Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ASTM D790 |
BLUESTAR 101G0 PBT Typical Applications: Appliance, partsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX1482T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC Copolymer, enhanced UV stabilization. Transprarent and tinted colors. Higher mold release content than SLX1432T.This data was supplied by SABIC-IP for the Europe-Africa-Middle E.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | |
Lehmann & Voss LUVOCOM® 1105-7825 PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
Unitika EX-1020K PA6, Dry Conducting nylonInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
SABIC Innovative Plastics NORYL ENG265 PPE+PS PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a.. |